Advantages of using Robot Micro Screws
2025,07,26
Common tearing and distorting forms of
Robot Micro Screws The stamping process of the intermediate protective bracket is: blanking punching--punching cut--flanging forming--cut--flanging.
There are various forms of tearing and distorting in the forming process of the intermediate protective bracket. The tearing parts are mainly distributed at the hole type of the workpiece, the junction of the R arc at the corner of the side wall and the wall neck, etc. Due to the differences in stamping forming and production process conditions, the proportion of each fracture part is different.
Tears can be one-time forming tears or tears caused by fatigue cracks, that is, invisible cracks.
Robot
Micro Screws were originally formed by stamping metal or non-metallic sheets with the help of the pressure of the press through stamping dies.
Robot Micro Screws are punched out under the premise of material consumption. The parts are heavy and have good rigidity. After the sheet is plastically deformed, the internal structure of the metal is improved, which improves the strength of Robot Micro Screws.
Robot Micro Screws have high dimensional accuracy, the same module size is uniform and consistent, and have good interchangeability. No further mechanical equipment processing is required to meet the general assembly and use requirements.
During the stamping process of Robot Micro Screws, since the surface of the raw material is not damaged, the surface quality is good and the surface is smooth and beautiful, which provides convenient conditions for surface painting, electroplating, phosphating and surface treatment.